1.1 This test method covers the determination of the coking value of tar and pitch having an ash content not over 0.5 %, as determined by Test Method D 2415.
1.2 Coking values by this test method are higher than those obtained by Test Method D 2416. See the bias statement in Section 13.
1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.