1.1 This practice covers procedures that can be followed to safeguard against the possible embrittlement of steel hot-dip galvanized after fabrication, and outlines test procedures for detecting embrittlement. Conditions of fabrication may induce a susceptibility to embrittlement in certain steels that can be accelerated by galvanizing. Embrittlement is not a common occurrence, however, and this discussion does not imply that galvanizing increases embrittlement where good fabricating and galvanizing procedures are employed. Where history has shown that for specific steels, processes and galvanizing procedures have been satisfactory, this history will serve as an indication that no embrittlement problem is to be expected for those steels, processes, and galvanizing procedures.