1.1 This practice covers the pressing and drying of chemically and nonchemically bonded aluminum-silicate and high alumina plastic and ramming mix refractory specimens classified in accordance with Classification C 673.
1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in parentheses are for information only.
1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.