1.1”This test method covers the determination of flexural strength, including stress-strain response, under monotonic loading of continuous fiber-reinforced advanced ceramic tubes at ambient temperature. This test method addresses tubular test specimen geometries, test specimen/grip fabrication methods, testing modes (force, displacement, or strain-control), testing rates (force rate, stress rate, displacement rate, or strain rate), and data collection and reporting procedures.