1.1 This test method covers the determination of the effect of perspiration on shoe upper leather. The leather is subjected to treatment with a formulation of artificial perspiration specific for breakdown of leather. Resistance to grain cracking as measured in accordance with Test Method D2210 and area loss are used as the criterion of deterioration. The artificial perspiration may also affect the flexibility of the leather. However, these effects have not been fully evaluated as criteria of deterioration in this test method. This test method does not apply to wet blue.

1.2 The values stated in inch-pound units are to be regarded as the standard. The values given in paretheses are provided for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Product Details

Published:
09/01/2005
Number of Pages:
2
File Size:
1 file , 57 KB
Redline File Size:
2 files , 110 KB