Click here to purchase

1.1 This practice provides procedures for estimating the percentage of wood failure that occurs in plywood-shear, block-shear, finger joint test specimens, or any other bondline involving wood.

1.2 The values stated in SI units are to be regarded as the standard. The values in parentheses are provided for information only.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.