1.1”This method describes the analysis of titanium and titanium alloys, such as specified by committee B10, by inductively coupled plasma atomic emission spectrometry (ICP-AES) and direct current plasma atomic emission spectrometry (DCP-AES) for the following elements:
Element |
Application |
Quantitative |
Aluminum |
0”’8 |
0.009 to 8.0 |
Boron |
0”’0.04 |
0.0008 to 0.01 |
Cobalt |
0-1 |
0.006 to 0.1 |
Chromium |
0”’5 |
0.005 to 4.0 |
Copper |
0”’0.6 |
0.004 to 0.5 |
Iron |
0”’3 |
0.004 to 3.0 |
Manganese |
0”’0.04 |
0.003 to 0.01 |
Molybdenum |
0”’8 |
0.004 to 6.0 |
Nickel |
0”’1 |
0.001 to 1.0 |
Niobium |
0-6 |
0.008 to 0.1 |
Palladium |
0-0.3 |
0.02 to 0.20 |
Ruthenium |
0-0.5 |
0.004 to 0.10 |
Silicon |
0”’0.5 |
0.02 to 0.4 |
Tantalum |
0-1 |
0.01 to 0.10 |
Tin |
0”’4 |
0.02 to 3.0 |
Tungsten |
0-5 |
0.01 to 0.10 |
Vanadium |
0”’15 |
0.01 to 15.0 |
Yttrium |
0”’0.04 |
0.001 to 0.004 |
Zirconium |
0”’5 |
0.003 to 4.0 |