1.1 This test method describes the inductively coupled plasma atomic emission spectrometric analysis of nickel alloys, such as specified by Committee B02, and having chemical compositions within the following limits:
Element |
Application Range (%) |
Aluminum |
0.01-1.00 |
Boron |
0.001-0.050 |
Calcium |
0.001-0.05 |
Carbon |
0.10-0.20 |
Chromium |
0.01-33.0 |
Cobalt |
0.10-20.0 |
Copper |
0.01-3.00 |
Iron |
0.01-50.0 |
Lead |
0.001-0.01 |
Magnesium |
0.0001-0.100 |
Manganese |
0.01-3.0 |
Molybdenum |
0.01-30.0 |
Niobium |
0.01-6.0 |
Nickel |
25.0-80.0 |
Nitrogen |
0.001-0.20 |
Oxygen |
0.0001-0.003 |
Phosphorous |
0.001-0.030 |
Sulfur |
0.0001-0.010 |
Silicon |
0.01-1.50 |
Tantalum |
0.005-0.10 |
Tin |
0.001-0.020 |
Titanium |
0.001-6.0 |
Tungsten |
0.01-5.0 |
Vanadium |
0.01-1.0 |
Zirconium |
0.01-0.10 |
Product Details
- Published:
- 01/01/2020
- Number of Pages:
- 10
- File Size:
- 1 file , 130 KB
- Redline File Size: